Sunday, October 28, 2007

Staining and tanning

What is the difference between staining and tanning?

There seems to be confusion among some photographers regarding the terms staining, and tanning, and the terms are often used interchangeably, probably because most staining developers are also tanning developers, and most tanning developers are also staining developers, but there are exceptions, and the two mechanisms perform very different, but highly complimentary functions in negative development.

Stain

Stain is the rock star of the staining/tanning duo, and gets most of the attention and press in the ultra-geeky photo community. The oxidation products of staining developers stain the film emulsion in proportion to exposure, meaning; more stain in the densest parts of the negative (highlights) than in the thinnest parts (shadows). The stain is useful because of its color as it relates to the spectral sensitivity of the printing paper. There are basically three sensitivity-types of printing papers: Graded silver papers, sensitive primarily to blue light, Variable Contrast papers, sensitive to Blue and Green light in various proportions, and Contact papers, which are sensitive to UV light. The effect of a stained negative on Graded silver papers, and Contact papers is essentially the same; to increase contrast. The effect of a stained negative on VC papers is more complicated, due to the Yellow Filter Effect of the stain image that creates an automatic split-filter effect with simultaneously reduced highlight contrast and increased shadow contrast.

A stained negative is a composite, composed of a silver image and a superimposed stain image that combine to create print density, and therein lays the magic! To achieve a given print density, less silver density is required, meaning less grain, because the stain has no grain. And since the stain density is added to the silver density, the total contrast potential of the negative is increased, meaning greater expansion potential, which is critical for long scale and self-masking UV contact printing processes. Stain density is also immune to the Callier Effect produced by condenser equipped enlargers, so stained negatives benefit all formats and printing processes.

Tanning

Tanning is the unsung hero of acutance. Tanning developers harden the emulsion in proportion to exposure, creating a relief image, and inhibiting the migration of the developer to the depths of the emulsion, and between areas of high and low densities, simultaneously reducing the appearance of grain and increasing apparent sharpness. Hardening is proportionally greater in the highlights than in the shadows, so shadow areas are developed to a greater depth in the emulsion, increasing emulsion speed by the compensating effect.

Synergy

Staining and tanning each deliver great advantages in film development, but in combination represent an almost magical set of characteristics that seem to defy conventional wisdom on the subject of developer formulation. It’s important to remember that conventional wisdom is based almost entirely on non-staining/tanning developer formulation, and very little has been written on the subject of staining/tanning developers over the last century, and much that has been written is ill informed or just plain nonsense, so when you’re told staining/tanning developers produce coarse grain, or give away emulsion speed to produce enhanced sharpness and tonality, so they’re only really good for large format contact printing, consider the mechanisms of staining and tanning and the benefits they confer to all formats.

Tuesday, January 2, 2007

Bella


This is my niece, Bella. I shot this last night, after dinner, with my XD-11/58mm f1.2.

Film: FP4+
Dilution: 1:100
Volume: 200ml
Time: 6:00
Temp: 70F
Agitation: Rotary
Scan: Neg

I haven't printed this image yet, but I had trouble with the contrast in the scan. I suspect it will print much better.

Thursday, December 28, 2006

Frederic Harster


This lovely image was made by Frederic Harster, and is posted here with his permission.

Film: Tri-X
Format 35mm
Dilution: 1:100
Time: 8:00
Temp: 20C/68F
Agitation: Rotary

Thank you, Fred.

Saturday, December 23, 2006

Frederic Harster Photos/ Neopan 400 test




Thank you Fred for sharing your data and images. Scanning is a subject about which I know very little and I appreciate the opportunity to learn from those more experienced than myself.

Data

Fuji Neopan 400

EI : 200
rotary process (CPE2+) @20°C
presoak : 5mn in distilled water
dev time : 8mn (1:100 - for 300ml total)
double fixing bath (4'/3')
wash in distilled water (20mn)

Negatives scanned

Thursday, December 21, 2006

Efke 25


This is photo of my beautiful niece, Bella, at Lake Lowell a few summers back. I was using my wife's Elan 7e and one of those 28-200 zoom lenses, handheld.

Film: Efke 25
Format: 35mm
EI: 25
Dilution: 1:100
Time: 6:00
Temp: 70F
agitation: 0:10/1:00

Sunday, December 17, 2006

Developing Kodak Technical Pan film


Kodak Technical Pan film is a specialized film not intended for pictorial photography, but with appropriate development is capable of excellent results in this application. 510-Pyro is especially well suited to this film, as it enhances sharpness through emulsion tanning and not increased graininess like other acutance developers do. With 510-Pyro the ultrafine grain of TP is retained, allowing enlargements of 20X or more without the appearance of grain, and the liquid smooth gradation of much larger formats.

To make 300ml of working solution, add 1 ml of 510-Pyro concentrate to 300ml of water at 70F, and stir. To make 600ml of working solution, add 2ml of 510-Pyro concentrate to 600ml of water at 70F, and stir. That’s all there is to it!

Optimum development time depends on the contrast of the scene photographed, among other things, so some compensation might be required for scenes of abnormally high or low contrast. For normal scenes, high quality negs can be made by developing TP in 510-Pyro as follows:

EI: 25-40
Dilution: 1:300
Time: 20:00
Temp: 70F
Agitation: continuous for first minute, and 10-15 sec at 10:00 (semi-stand)

Increased agitation frequency will require a corresponding reduction in development time. For normal intermittent development with agitation at 10 sec./minute, develop for 16 minutes.

Saturday, December 16, 2006

Printing stained negatives with VC papers

I'm working on an article describing the special considerations regarding the printing of stained negatives with VC papers, and will post the article here when complete. I hope users of staining developers find it useful.

Jay